Sample
Name
Pellet of Cu mixed with BN
Date
2023-02-16
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Mass
0.3001 ± 0.0004 g
Temperature
300.0 ± 1.0 K
Temperature max
293.15 K
Pressure
1.0 ± 0.001 bar
Title
mixing and compressing Cu with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Cu mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min