Sample
Name
Pellet of Tl2S mixed with BN
Date
2015-06-21
Provider
Prolabo
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Mass
0.027 g
Temperature
15.0 ± 5.0 K
Type
atomic gas
Fluids
Fluid temperature
15.0 K
Fluid pressure
1.0 bar
Title
mixing and compressing Tl2S with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Tl2S mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min