Sample
Name
Pellet of natural eudialyte Na4(Ca,Ce,Fe,Mn,Y,La,Sr,K)3ZrSi8O22(OH,Cl)2 mixed with BN
Date
2009-11-01
Provider
Poudrette Quary - Mount St-Hilaire - Canada
Thickness
1.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Temperature
293.0 $\pm$ 5.0 $K$
Temperature max
293.0 $K$
Type
ambient air
Fluid temperature
293.0 $K$
Fluid pressure
1.0 $bar$
Title
mixing and compressing of natural eudialyte Na4(Ca,Ce,Fe,Mn,Y,La,Sr,K)3ZrSi8O22(OH,Cl)2 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of natural eudialyte Na4(Ca,Ce,Fe,Mn,Y,La,Sr,K)3ZrSi8O22(OH,Cl)2 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed BN and eudialyte manually in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min