Sample
Name
IDP L2083 B7
Date
2023-01-01
Provider
Institut d'Astrophysique Spatial, Orsay, France
Thickness
3.0 $\pm$ 0.5 ${\mu}m$
Substrate material
Diamond
Comments
Grain crushed inside a diamond compression cell
Temperature
20.0 $\pm$ 10.0 $^{\circ}C$
Temperature max
30.0 $\pm$ 5.0 $^{\circ}C$
Type
ambient air
Fluid temperature
20.0 $\pm$ 10.0 $^{\circ}C$
Fluid pressure
1.0 $atm$
Number
1
Layers
Title
IDP 2083 B7 preparation

Precursors

Matters

Produced sample

Sample
IDP L2083 B7 (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 during layer formation 2014-01-01 mechanical mechical crushing of the IDP L2083 B7 in the diamond compression cell
Comments
The sample was crushed into a diamond compression cell until obtain a maximum thickness of 3 µm.