- Database
 - Experimentalists
 
- Date
 - 2012-04-06
 - Provider
 - IPAG, Pierre Beck
 
- Thickness
 - 0.8 ± 0.01 mm
 - Diameter
 - 13.0 mm
 - Mass
 - 0.301 ± 0.0015 g
 - Substrate material
 - sample holder in aluminium with a centered hole to hold the pellet
 - Comments
 - KBr pellet of 13mm of diameter and 0.8mm thick
 
- Temperature
 - 22.0 ± 2.0 ∘C
 - Temperature max
 - 22.0 ± 2.0 ∘C
 
- Type
 - vacuum
 - Fluid pressure
 - 0.001 mbar
 - Comments
 - stored in a dessicator
 
- Number
 - 1
 - Layers
 - 
                    
- WIS91600 meteorite pellet , 0.8 mm
 
 
- Title
 - Grinding of the WIS91600 matter, mixing with Kbr, pellet making
 - Matters
 - Sample
 - WIS91600 meteorite pellet Tamb (this sample)
 - Processing steps
 - 
                    
Step Chronology Date Type Process Changes #1 before layer formation 2012-04-06 mechanical grinding bulk meteorite reduced to grains with size lower than 10 microns #2 before layer formation 2012-04-06 thermal 300 mg of commercial ultrapure KBr powder was heated under ambient air to 80°C overnight (~10h) removal of adsorbed/hydration water in KBr powder #3 before layer formation 2012-04-06 mixing homogeneous mixing 1.0 mg of grinded meteorite was weighed and mixed with 300 mg of dried commercial ultrapure KBr powder #4 before layer formation 2012-04-06 pressure pressure formation of a pellet of 13mm diameter and 0.8 mm thick under 400 bar of pressure