Sample
Name
Pellet of AgO mixed with BN
Date
2013-01-01
Thickness
1.0 ± 0.5 mm
Diameter
5.0 mm
Mass
0.023 ± 0.006 g
Temperature
293.0 ± 5.0 K
Temperature max
293.0 K
Type
ambient air
Fluid temperature
293.0 K
Fluid pressure
1.0 bar
Title
mixing and compressing of AgO with BN

Precursors

Matters

Produced sample

Sample
Pellet of AgO mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed BN and AgO manually in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min