Sample
Name
Pellet of cadmium oxide mixed with BN
Date
2005-01-01
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Temperature
15.0 $\pm$ 5.0 $K$
Temperature max
293.0 $K$
Type
atomic gas
Fluids
Fluid temperature
15.0 $K$
Title
mixing and compressing cadmium oxide with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of cadmium oxide mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min