Sample
Name
Pellet of V2O4 mixed with BN
Date
2006-03-04
Provider
Sigma-Aldrich
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Mass
1.0039 ± 0.0011 g
Title
mixing and compressing V2O4 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of V2O4 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min