Sample
Name
Pellet of PtO2 mixed with BN
Date
2018-11-12
Provider
Thermofisher
Thickness
2.0 0.5
Diameter
5.0
Mass
101.3
Temperature
25.0 -268.1
Temperature max
19.85
Title
mixing and compressing PtO2 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of PtO2 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min