Sample
Name
Pellet of Cavansite mineral of V(IV), (Ca(VO)Si4O10.4H2O mixed with BN
Date
2004-09-01
Provider
Carion (https://carionpluscarion.fr/fr/12-mineraux)
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
0.1029 $g$
Temperature
20.0 $\pm$ 5.0 $^{\circ}C$
Temperature max
20.0 $^{\circ}C$
Type
ambient air
Fluid temperature
20.0 $^{\circ}C$
Fluid pressure
1.0 $bar$
Title
mixing and compressing Cavansite mineral of V(IV), (Ca(VO)Si4O10.4H2O with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Cavansite mineral of V(IV), (Ca(VO)Si4O10.4H2O mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min