Sample
Name
Pellet of Gd2Si2O7 mixed with BN
Date
2015-05-04
Provider
laboratory synthesis (Marion Louvel) at the ANU
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Type
ambient air
Fluid temperature
300.0 K
Fluid pressure
1.0 bar
Title
mixing and compressing Gd2Si2O7 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Gd2Si2O7 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min