Sample
Name
MAC87320 matrix grains (CR) on diamond
Date
2021-01-01
Provider
IPAG
Thickness
15.0 $\pm$ 5.0 ${\mu}m$
Diameter
40.0 ${\mu}m$
Substrate material
diamond window
Substrate comments
diamond window of 3.5mm diameter
Comments
manual selection under binocular of about 10 matrix grains of approximate diameter between 30 and 50 microns
Temperature
22.0 $\pm$ 2.0 $^{\circ}C$
Temperature max
22.0 $\pm$ 2.0 $^{\circ}C$
Type
ambient air
Fluid temperature
22.0 $\pm$ 2.0 $^{\circ}C$
Fluid pressure
1.0 $atm$
Number
1
Layers
Title
selection and preparation of the matrix grains on diamond windows

Precursors

Matters

Produced sample

Sample
MAC87320 matrix grains (CR) on diamond (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2021-01-01 mechanical Manual selection under optical binocular of about 10 matrix grains of about 30-50 microns diameter. Matrix selected based on its black color and on its fine-grained texture
#2 during layer formation 2021-01-01 mechanical Grains pressed between two diamond windows with a mechanical press grain crushed down to a thickness of about 10 microns