Sample
Name
Pellet of Cs2O4S mixed with BN
Date
2024-05-03
Provider
Sigma-Aldrich (Cesium Sulfate 230030)
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Mass
0.0427 ± 0.001 g
Type
ambient air
Fluid temperature
300.0 K
Fluid pressure
1.0 bar
Title
mixing and compressing Cs2O4S with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Cs2O4S mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min